Copper Alloy Achieves Superalloy-Like Strength | Technology Networks
Complete the form below to unlock access to ALL audio articles.
A team of researchers from Arizona State University, the U.S. Army Research Laboratory, Lehigh University and Louisiana State University has developed a groundbreaking high-temperature copper alloy with exceptional thermal stability and mechanical strength.
The research team’s findings on the new copper alloy, published in the prestigious journal Science, introduce a novel bulk Cu-3-Ta-0.5Li nanocrystalline alloy that exhibits remarkable resistance to coarsening and creep deformation, even at temperatures near its melting point.
“Our alloy design approach mimics the strengthening mechanisms found in Ni-based superalloys,” said Kiran Solanki, a professor at the Ira A. Fulton Schools of Engineering in the School for Engineering of Matter, Transport and Energy and a co-author of the study.
Currently, nickel-based superalloys, known for their exceptional strength, corrosion resistance and high-temperature stability, are the primary material used in applications where these properties are critical, such as aerospace components, gas turbine engines and chemical processing equipment.
New materials are especially needed throughout the aerospace and defense industries — think of the strength, durability and heat resistance needed for high-speed flight or deploy weaponry. This spurs the research community to continue to push the boundaries of high-impact technologies.
“We have to critically think about what we can do to solve engineering problem in a more outside-the-box way,” Solanki said. “At the end of the day, I'm more curious about what I don't know.”
Subscribe to Technology Networks’ daily newsletter, delivering breaking science news straight to your inbox every day.
Solanki's main research interests investigate the structure and property relationships of advanced materials across multiple length scales. His goal is to manufacture advanced, multifunctional materials for extreme applications including radiation, high rate, fatigue and prevention of slow deformation under mechanical stresses, or creep.
“When we look inside our body, we try to look for fingerprints of cell mutation for cancer,” Solanki said. “Similarly, structural materials have a unique fingerprint when they are subjected to any event like radiation or heat. They will leave behind a fingerprint which causes them to fail or not to perform the way they should perform.”
The newly engineered alloy owes its superior properties to a unique nanoscale structure featuring precisely ordered copper lithium precipitates surrounded by a tantalum-rich atomic bilayer. The addition of precisely half a percent of lithium — no more, no less — to the previously immiscible Cu-Ta system alters the precipitate morphology. It changes the sphere-like precipitate in Cu-Ta system into forming stable cuboidal structures that significantly enhance thermal and mechanical performance.
“And in this case, having a copper lithium precipitate with a stable bilayer of Ta is when we can alter high temperature fingerprint for failure,” Solanki said. “By manipulating fingerprints, we have developed a copper alloy that maintains its strength and structural integrity even after prolonged exposure to high temperatures.”
Key findings from the copper superalloy research include:
The discovery opens new avenues for the development of next-generation copper alloys for applications in aerospace, energy and defense industries. Potential uses include heat exchangers, high-performance electrical components, weaponry and structural materials requiring durability in extreme conditions.
“This research not only advances our understanding of alloy design but also paves the way for materials that can withstand extreme environments,” said Kris Darling, another Army Research Laboratory co-author of the study. “The manipulation of fingerprints through nanostructuring in alloy could revolutionize the way we approach high-temperature material development.”
Reference: Hornbuckle BC, Smeltzer JA, Sharma S, et al. A high-temperature nanostructured Cu-Ta-Li alloy with complexion-stabilized precipitates. Science. 2025;387(6741):1413-1417. doi: 10.1126/science.adr0299
This article has been republished from the following materials. Note: material may have been edited for length and content. For further information, please contact the cited source. Our press release publishing policy can be accessed here.