Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni

Specification
SHARE

Description

Basic Info.
Model NO. Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632
Special Use Chemical and Petrochemical Processing
Application Superheater and Reheater Pipes in Power Plants
Transport Package Standard Sea-Worthy Package or as Required
Specification Diameter: 4-50mm
Trademark Hengrui
Origin Made in China
Production Capacity 50000 Tons Annually
Product Description

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni-Cr-Co-Based Precipitation Hardening Wrought Superalloy

Specification
Product NameNickel Alloy
MaterialMonel/Inconel/Hastelloy/Duplex Steel/PH Steel/Nickel Alloy
ShapeRound,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet
GradeDuplex: 2205(UNS S31803/S32205),2507(UNS S32750),UNS S32760(Zeron 100),2304,904L
Others:253Ma,254SMo,654SMo,F50(UNSS32100)F60,F61,F65,1J22,N4,N6 etc.
Alloy : Alloy 20/28/31
Hastelloy:HastelloyB-2/B-3/C22/C-4/S/C276/C-2000/G-35/G-30/X/N/g
Hastelloy B/UNS N10001,Hastelloy B-2/UNS N10665/DIN W.Nr.2.4617,Hastelloy C
Hastelloy C-4/UNS N06455/DIN W.Nr.2.4610,Hastelloy C-22/UNS N06022/DIN W.Nr.2.4602
Hastelloy C-276/UNS N10276/DIN W.Nr.2.4819,Hastelloy X/UNS N06002/DIN W.Nr.2.4665
Haynes: Haynes 230/556/188
Inconel 600/601/602CA/617/625/713/718/738/X-750,Carpenter 20
Inconel 718/UNS N07718/DIN W.Nr.2.4668, Inconel 601/UNS N06601/DIN W.Nr.2.4851
Inconel 625/UNS N06625/DIN W.Nr.2.4856, Inconel 725/UNS N07725, Inconel X-750/UNS N07750/DIN W.Nr.2.4669, Inconel 600/UNS N06600/DIN W.Nr.2.4816
Incoloy: Incoloy 800/800H/800HT/825/925/926
GH: GH2132,GH3030,GH3039,GH3128,GH4180,GH3044
Monel: Monel 400/K500/R405
Nitronic: Nitronic 40/50/60
Nimonic: Nimonic 75/80A/90/A263
SpecificationWire: 0.01-10mm
Strip: 0.05*5.0-5.0*250mm
Bar: φ4-50mm;Length 2000-5000mm
Pipe: φ6-273mm;δ1-30mm;Length 1000-8000mm
Sheet: δ0.8-36mm;Width 650-2000mm;Length 800-4500mm
Product Characteristics1.According to the preparation process can be divided into deformation superalloys,
casting superalloys and powder metallurgysuperalloys
2.According to the strengthening mode, there are solid solution strengthening type, precipitation strengthening type, oxidedispersion strengthening type and fiber strengthening type, etc.
StandardGB,AISI,ASTM,DIN,EN,SUS,UNS etc.
InspectionISO,SGS,BV etc.
ApplicationHigh temperature components such as turbine blades, guide vanes, turbine disks, high pressure compressor disks, machinemanufacturing and combustion chambers used in the manufacture of aviation, naval andindustrial gas turbines
Packaging1. Wooden cases
2. Paper
3. Plastic
4. Foam or other requirements
DeliveryDepends on the specifications, quantity and etc.
PaymentT/T,L/C etc.

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni-Cr-Co-Based Precipitation Hardening Wrought Superalloy

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni-Cr-Co-Based Precipitation Hardening Wrought Superalloy

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni-Cr-Co-Based Precipitation Hardening Wrought Superalloy

Gh4090 / Gh90 / Nimonic90 / Uns N07090 / 2.4632 / Precipitation Hardening Deformed Superalloy / Ni-Cr-Co-Based Precipitation Hardening Wrought Superalloy

Our Contact