Wrought Superalloy Inconel 625 Inconel 738 Gh4169 Gh5605
RFQ Q: Are you trading company or manufacturer ?A: We are factory/manufacture.Q: How long is your delivery time?A: Gener
Description
Basic Info.
Elongation (Min %) | 30 |
Transport Package | Wooden Case/Pallet |
Specification | Wall thickness 0.08-3.0mm. width 5.0-420mm. |
Trademark | shengpo |
Origin | China |
HS Code | 75062000 |
Production Capacity | 5 Tons Per Month |
Product Description
Grade | Thickness(mm) | Allowable Thickness Deviation(mm) | Test temperature | HVHV(Hardness) | |
General precision | High Precision | ||||
GH5188 GH5605 GH738 | 0.25<T≤0.6 | +/-0.015 | +/-0.01 | 23ºC | GH5188 239/234/239 |
GH5605 262/260/267 | |||||
0.6<T≤1.0 | +/-0.020 | +/-0.015 | |||
+/-0.030 | +/-0.020 | ||||
1.0<T≤2.0 | |||||
Solid solution strengthened cobalt base superalloy with 14% - 15% tungsten solid solution strengthening makes the alloy have excellent high temperature thermal strength. Adding high content of chromium and trace lanthanum, the alloy has good high temperature oxidation resistance, satisfactory molding and welding process performance. It is suitable for manufacturing combustion chamber and guide vane of aeroengine, and high temperature parts with high oxidation resistance Application scope: aero engine combustion chamber, guide vane, high temperature parts, etc., can also be made into thin plate, strip, etc |
A: We are factory/manufacture
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 45-90 days if the goods are not in stock, it is according to quantity
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight
Q: What is your terms of payment ?
A: 30% T/T in advance ,balance before shippment or BL at sight.
Prev: Powerful Production Capacity Superalloy Gh5188 Gh5605 High Precision Bt800mo
Next: Gh4033 Nicke Tube Superalloy with Sufficient High Temperature Strength M36
Our Contact
Send now